Optical constants of SUMITA - PSK (Dense phosphate crown)
K-PSK500(M)
Wavelength:
µm
(0.270 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.3725199-0.0067756972λ^{2}+0.01066551λ^{-2}+0.00018548975λ^{-4}-5.7674134\text{×}10^{-06}λ^{-6}+3.2946743\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.34e-05 6.83e-09 1.81e-11 3.74e-07 5.55e-10 0.195 nd: 1.55000 Vd: 71.9 glass_code: 552720 density: 3.76 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.08e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.29e-05 K-1 dPgF: 0.0178 climatic_resistance: 1.0 acid_resistance: 2.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book