Optical constants of SUMITA - PSK (Dense phosphate crown)
K-PSK200(M)
Wavelength:
µm
(0.290 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5524515-0.0088629121λ^{2}+0.014923738λ^{-2}+0.00026036731λ^{-4}-2.7057207\text{×}10^{-06}λ^{-6}+4.8084913\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.04e-06 8.75e-09 -5.81e-11 5.61e-07 7.53e-10 0.187 nd: 1.61083 Vd: 58.9 glass_code: 613590 density: 3.38 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.23e-05 K-1 dPgF: 0.0029 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book