Optical constants of SUMITA - PSF
K-PSFn215
Wavelength:
µm
(0.4 – 2.000)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=4.2994108-0.014091413λ^{2}+0.097855062λ^{-2}+0.0076857652λ^{-4}-0.00046786841λ^{-6}+0.00012218724λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.64e-05 4.6e-08 -2.91e-10 3.47e-06 -3e-09 0.301 nd: 2.15400 Vd: 17.2 glass_code: 154172 density: 7.1 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.01e-05 K-1 dPgF: 0.0498 climatic_resistance: 1.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book