Optical constants of SUMITA - PSF
K-PSFn214(M)
Wavelength:
µm
(0.4 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=4.2564848-0.015091057λ^{2}+0.086600358λ^{-2}+0.011001775λ^{-4}-0.0012680564λ^{-6}+0.00017404024λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.6e-05 2.83e-08 -1.6e-10 3.11e-06 2.04e-09 0.316 nd: 2.13909 Vd: 17.7 glass_code: 144178 density: 7.06 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.8e-06 K-1 dPgF: 0.0457 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book