Optical constants of SUMITA - PSF
K-PSFn202(M)
Wavelength:
µm
(0.390 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.8290543-0.016470594λ^{2}+0.065112852λ^{-2}+0.0059865818λ^{-4}-0.00053116084λ^{-6}+7.8076366\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.41e-05 2.66e-08 -5.37e-10 2.35e-06 1.36e-09 0.301 nd: 2.01365 Vd: 21.4 density: 6.22 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.4e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.6e-06 K-1 dPgF: 0.0289 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book