Optical constants of SUMITA - PSF
K-PSFn173
Wavelength:
µm
(0.4 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=4.2785429-0.014012371λ^{2}+0.096019323λ^{-2}+0.0077567166λ^{-4}-0.00051560398λ^{-6}+0.00012285966λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.59e-05 2.25e-08 -1.48e-10 3.28e-06 3.23e-09 0.333 nd: 2.14780 Vd: 17.3 glass_code: 148173 density: 7.03 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.7e-06 K-1 dPgF: 0.0481 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book