Optical constants of SUMITA - PSF
K-PSFn1(M)
Wavelength:
µm
(0.380 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.418365-0.015830577λ^{2}+0.056024892λ^{-2}+0.0042907055λ^{-4}-0.00027089374λ^{-6}+4.8560287\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.11e-06 1.75e-08 -2.81e-10 1.25e-06 1.62e-09 0.307 nd: 1.89945 Vd: 21.3 glass_code: 907212 density: 4.15 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.4e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.02e-05 K-1 dPgF: 0.0238 climatic_resistance: 1.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book