Optical constants of SUMITA - PSF
K-PSFn1

Wavelength: µm
 (0.380 – 2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.4407637-0.015750622λ^{2}+0.059024249λ^{-2}+0.0035647556λ^{-4}-0.00012641103λ^{-6}+4.0309245\text{×}10^{-05}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -3.11e-06 1.75e-08 -2.81e-10 1.25e-06 1.62e-09 0.307
nd: 1.90680
Vd: 21.2
glass_code: 907212
density: 4.15 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 7.4e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.02e-05 K-1
dPgF: 0.0245
climatic_resistance: 1.0
acid_resistance: 1.0

References

SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SUMITA Optical Glass, Inc.

SUMITA Optical Glass, Inc. is a Japanese glass manufacturer