Optical constants of SUMITA - PMK
K-PMK30(M)

Wavelength: µm
 (0.280 – 2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.2835931-0.0098380554λ^{2}+0.010317986λ^{-2}-3.5867157\text{×}10^{-06}λ^{-4}+2.1079335\text{×}10^{-05}λ^{-6}-1.145809\text{×}10^{-06}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 3.49e-07 1.51e-08 -7.35e-11 3.65e-07 5.07e-10 0.174
nd: 1.52002
Vd: 70.2
glass_code: 525704
density: 2.6 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 8.3e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 8.7e-06 K-1
dPgF: 0.0069
climatic_resistance: 2.0
acid_resistance: 1.0

References

SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SUMITA Optical Glass, Inc.

SUMITA Optical Glass, Inc. is a Japanese glass manufacturer

External links


Glass

External links