Optical constants of SUMITA - PMK
K-PMK30
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.2984199-0.0098977917λ^{2}+0.010454435λ^{-2}-1.1762246\text{×}10^{-05}λ^{-4}+2.220678\text{×}10^{-05}λ^{-6}-1.2212713\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.49e-07 1.51e-08 -7.35e-11 3.65e-07 5.07e-10 0.174 nd: 1.52500 Vd: 70.4 glass_code: 525704 density: 2.6 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.7e-06 K-1 dPgF: 0.0062 climatic_resistance: 2.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book