Optical constants of SUMITA - PG
K-PG395(M)

Wavelength: µm
 (0.340 – 2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.6598043-0.0097241142λ^{2}+0.023341531λ^{-2}+0.0010595162λ^{-4}-4.9515252\text{×}10^{-05}λ^{-6}+7.5464331\text{×}10^{-06}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -1.15e-05 1.65e-09 -6.23e-11 1.13e-06 1.19e-09 0.255
nd: 1.65296
Vd: 36.8
glass_code: 658369
density: 3.5 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 1.24e-05 K-1
  - temperature_range: 20 300 °C
    coefficient: 1.59e-05 K-1
dPgF: 0.0057
climatic_resistance: 1.0
acid_resistance: 3.0

References

SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SUMITA Optical Glass, Inc.

SUMITA Optical Glass, Inc. is a Japanese glass manufacturer

External links


Glass

External links