Optical constants of SUMITA - PG
K-PG395
Wavelength:
µm
(0.340 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.6754764-0.0097406258λ^{2}+0.023844634λ^{-2}+0.00098091134λ^{-4}-3.8466006\text{×}10^{-05}λ^{-6}+6.9920317\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.15e-05 1.65e-09 -6.23e-11 1.13e-06 1.19e-09 0.255 nd: 1.65800 Vd: 36.9 glass_code: 658369 density: 3.5 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.24e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.59e-05 K-1 dPgF: 0.0049 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)