Optical constants of SUMITA - PG
K-PG375
Wavelength:
µm
(0.300 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.345943-0.0077317211λ^{2}+0.011783664λ^{-2}+0.00025239185λ^{-4}-1.2352344\text{×}10^{-05}λ^{-6}+8.7540057\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.51e-05 1.45e-09 -9.02e-11 5.44e-07 3.99e-10 0.176 nd: 1.54250 Vd: 62.9 glass_code: 543629 density: 2.9 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.29e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.6e-05 K-1 dPgF: 0.0036 climatic_resistance: 2.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book