Optical constants of SUMITA - PG
K-PG325(M)
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.2385136-0.0070158219λ^{2}+0.0095692073λ^{-2}+0.00018606584λ^{-4}-8.4285475\text{×}10^{-06}λ^{-6}+5.3174439\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.86e-05 -3.2e-09 -2.53e-11 4.98e-07 8.02e-10 0.172 nd: 1.50506 Vd: 70.4 glass_code: 507705 density: 3.0 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.43e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.65e-05 K-1 dPgF: 0.0122 climatic_resistance: 1.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book