Optical constants of SUMITA - PFK
K-PFK85(M)
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.180434-0.0050369414λ^{2}+0.007415342λ^{-2}+0.000191031λ^{-4}-1.3017551\text{×}10^{-05}λ^{-6}+6.1457339\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -2.28e-05 -1.71e-09 6.72e-11 3.39e-07 4.74e-10 0.176 nd: 1.48375 Vd: 85.0 glass_code: 486852 density: 3.97 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.29e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.63e-05 K-1 dPgF: 0.0388 climatic_resistance: 1.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book