Optical constants of SUMITA - PBK
K-PBK40(M)
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.2666695-0.010697246λ^{2}+0.010455014λ^{-2}+0.00024731938λ^{-4}-9.4216199\text{×}10^{-06}λ^{-6}+3.3360125\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.91e-06 2.06e-08 1.52e-11 4.18e-07 1.61e-10 0.165 nd: 1.51497 Vd: 63.3 glass_code: 518635 density: 2.39 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.4e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.3e-06 K-1 dPgF: -0.0035 climatic_resistance: 2.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book