Optical constants of SUMITA - LaSF (Lanthanum dense flint)
K-LaSFn8
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.2767321-0.015115573λ^{2}+0.030753445λ^{-2}+0.00078350578λ^{-4}-3.4594495\text{×}10^{-06}λ^{-6}+2.0542573\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.92e-06 1.65e-08 -2.32e-10 6.04e-07 6.91e-10 0.225 nd: 1.83500 Vd: 42.7 glass_code: 835427 density: 4.9 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.4e-06 K-1 dPgF: -0.0093 climatic_resistance: 1.0 acid_resistance: 2.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)