Optical constants of SUMITA - LaSF (Lanthanum dense flint)
K-LaSFn2
Wavelength:
µm
(0.320 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1666472-0.014823032λ^{2}+0.030366123λ^{-2}+0.0010942894λ^{-4}-4.2108569\text{×}10^{-05}λ^{-6}+5.7186779\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 5.26e-06 1.83e-08 -3.28e-10 7.62e-07 8.92e-10 0.222 nd: 1.80500 Vd: 39.6 glass_code: 805396 density: 4.13 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7e-06 K-1 dPgF: -0.0066 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book