Optical constants of SUMITA - LaSF (Lanthanum dense flint)
K-LaSFn10
Wavelength:
µm
(0.340 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.2128137-0.015587464λ^{2}+0.028249299λ^{-2}+0.00086439607λ^{-4}-2.9175496\text{×}10^{-05}λ^{-6}+2.9912535\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 3.02e-06 1.34e-08 -1.66e-10 6.41e-07 6.88e-10 0.194 nd: 1.81550 Vd: 44.4 glass_code: 816444 density: 4.8 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.2e-06 K-1 dPgF: -0.0105 climatic_resistance: 1.0 acid_resistance: 2.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book