Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaKn5
Wavelength:
µm
(0.330 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.6761221-0.012108757λ^{2}+0.016143507λ^{-2}+0.00051920927λ^{-4}-2.8395319\text{×}10^{-05}λ^{-6}+1.8554978\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -8.68e-07 1.28e-08 -1.92e-10 5.01e-07 9.91e-10 0.169 nd: 1.65000 Vd: 55.8 glass_code: 650558 density: 3.71 g/cm3 thermal_expansion: - temperature_range: 20 300 °C coefficient: 8e-06 K-1 dPgF: -0.0011 climatic_resistance: 2.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book