Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaKn4
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.744955-0.013026744λ^{2}+0.016661518λ^{-2}+0.00048278001λ^{-4}-2.5815825\text{×}10^{-05}λ^{-6}+1.5241247\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.88e-06 1.19e-08 -1.1e-10 3.48e-07 6.14e-10 0.223 nd: 1.67100 Vd: 57.2 glass_code: 671572 density: 3.88 g/cm3 thermal_expansion: - temperature_range: 20 300 ℃ coefficient: 8.5e-06 K-1 dPgF: -0.0038 climatic_resistance: 2.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book