Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaKn2
Wavelength:
µm
(0.290 – 2.000)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.6498456-0.013078949λ^{2}+0.014887079λ^{-2}+0.0003621869λ^{-4}-1.1506273\text{×}10^{-05}λ^{-6}+6.1300945\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.24e-06 1.48e-08 -2.56e-10 3.66e-07 4.69e-10 0.182 nd: 1.64050 Vd: 60.1 glass_code: 641601 density: 3.66 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 8e-06 K-1 dPgF: -0.0029 climatic_resistance: 1.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book