Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaK8
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8797142-0.015009518λ^{2}+0.01933782λ^{-2}+0.00048379963λ^{-4}-1.1367908\text{×}10^{-05}λ^{-6}+7.0484275\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 9.91e-07 1.3e-08 -2.26e-10 5.21e-07 4.99e-10 0.162 nd: 1.71300 Vd: 53.9 glass_code: 713539 density: 3.79 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 4.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.5e-06 K-1 dPgF: -0.0065 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book