Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaK7
Wavelength:
µm
(0.290 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.6835737-0.012086498λ^{2}+0.015193489λ^{-2}+0.00064847987λ^{-4}-5.2423893\text{×}10^{-05}λ^{-6}+2.8301452\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.13e-06 1.62e-08 -5.04e-11 3.71e-07 6.15e-10 0.214 nd: 1.65160 Vd: 58.3 glass_code: 652583 density: 3.76 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.4e-06 K-1 dPgF: -0.0021 climatic_resistance: 2.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)