Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaK14
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8277206-0.013838479λ^{2}+0.0179847λ^{-2}+0.00057777884λ^{-4}-3.7712827\text{×}10^{-05}λ^{-6}+2.2935918\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -4.5e-07 1.44e-08 -3.03e-10 5.54e-07 7.23e-10 0.135 nd: 1.69680 Vd: 55.6 glass_code: 697556 density: 3.64 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.4e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.1e-06 K-1 dPgF: -0.0065 climatic_resistance: 1.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book