Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaK11
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.703071-0.011555097λ^{2}+0.016440907λ^{-2}+0.00044044678λ^{-4}-2.1866961\text{×}10^{-05}λ^{-6}+1.3531002\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -2.69e-06 1.38e-08 -5.45e-11 4.86e-07 7.71e-10 0.155 nd: 1.65830 Vd: 57.3 glass_code: 658573 density: 3.85 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.5e-06 K-1 dPgF: -0.004 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book