Optical constants of SUMITA - LaFK
K-LaFK60
Wavelength:
µm
(0.270 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.6248172-0.010251149λ^{2}+0.0143793λ^{-2}+0.00024017461λ^{-4}-1.041901\text{×}10^{-06}λ^{-6}+1.0237991\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -9.6e-06 1.03e-08 -7.48e-11 3.87e-07 1.56e-10 0.188 nd: 1.63246 Vd: 63.8 glass_code: 632638 density: 4.29 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 1.14e-05 K-1 dPgF: 0.0041 climatic_resistance: 1.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book