Optical constants of SUMITA - LaFK
K-LaFK58(M)
Wavelength:
µm
(0.270 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8101512-0.012726602λ^{2}+0.017535146λ^{-2}+0.00035913422λ^{-4}-8.8851874\text{×}10^{-06}λ^{-6}+6.1852602\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -4.73e-06 9.33e-09 -1.14e-10 4.36e-07 4.83e-10 0.169 nd: 1.69097 Vd: 58.4 glass_code: 696590 density: 4.56 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.9e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.3e-06 K-1 dPgF: -0.0029 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)