Optical constants of SUMITA - LaFK
K-LaFK55(M)
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8008078-0.013188685λ^{2}+0.01809632λ^{-2}+0.00040852782λ^{-4}-1.2855113\text{×}10^{-05}λ^{-6}+1.0513058\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -2.43e-06 1.08e-08 -8.1e-11 5.36e-07 6.73e-10 0.111 nd: 1.68875 Vd: 55.8 glass_code: 694563 density: 4.34 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.1e-06 K-1 dPgF: -0.0041 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book