Optical constants of SUMITA - LaFK
K-LaFK50(M)
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.0568421-0.011998981λ^{2}+0.024194996λ^{-2}+0.0004815051λ^{-4}+2.2084112\text{×}10^{-06}λ^{-6}+4.3040075\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -3.11e-07 1.35e-08 -2.34e-10 5.76e-07 8.89e-10 0.201 nd: 1.76831 Vd: 49.7 glass_code: 772500 density: 5.2 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9e-06 K-1 dPgF: -0.0056 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book