Optical constants of SUMITA - LaFK
K-LaFK50
Wavelength:
µm
(0.280 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.070131-0.012037535λ^{2}+0.023978866λ^{-2}+0.00056153238λ^{-4}-1.0529871\text{×}10^{-05}λ^{-6}+1.1710915\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.11e-07 1.35e-08 -2.34e-10 5.76e-07 8.89e-10 0.201 nd: 1.77200 Vd: 50.0 glass_code: 772500 density: 5.2 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 9e-06 K-1 dPgF: -0.0051 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book