Optical constants of SUMITA - LaF (Lanthanum flint)
K-LaFn3
Wavelength:
µm
(0.340 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.827081-0.010220727λ^{2}+0.021224097λ^{-2}+0.0006653956λ^{-4}-3.3316539\text{×}10^{-05}λ^{-6}+3.16429\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.22e-06 1.12e-08 -3.14e-10 6.46e-07 6.47e-10 0.204 nd: 1.70000 Vd: 48.0 glass_code: 700480 density: 4.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.6e-06 K-1 dPgF: -0.0034 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book