Optical constants of SUMITA - GFK
K-GFK68

Wavelength: µm
 (0.280 – 2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.4994867-0.0059285872λ^{2}+0.012743526λ^{-2}+0.00015469636λ^{-4}+3.9947612\text{×}10^{-06}λ^{-6}-1.760356\text{×}10^{-07}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -2.36e-05 2.85e-09 4.82e-11 4.01e-07 2.74e-10 0.183
nd: 1.59240
Vd: 68.3
glass_code: 592683
density: 4.51 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 1.29e-05 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.52e-05 K-1
dPgF: 0.0179
climatic_resistance: 1.0
acid_resistance: 1.0

References

SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SUMITA Optical Glass, Inc.

SUMITA Optical Glass, Inc. is a Japanese glass manufacturer

External links


Glass

External links