Optical constants of SUMITA - CSK
K-CSK120(M)
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.4722418-0.01073376λ^{2}+0.013736108λ^{-2}+0.00027440551λ^{-4}-9.8995396\text{×}10^{-06}λ^{-6}+8.2295122\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.46e-06 1.54e-08 -2.77e-11 5.04e-07 3.24e-10 0.172 nd: 1.58445 Vd: 59.2 glass_code: 587596 density: 3.0 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.2e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.1e-06 K-1 dPgF: -0.0038 climatic_resistance: 2.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book