Optical constants of SUMITA - CSK
K-CSK120
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.4804566-0.01071977λ^{2}+0.0135632λ^{-2}+0.00034918608λ^{-4}-2.3041786\text{×}10^{-05}λ^{-6}+1.5937217\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.46e-06 1.54e-08 -2.77e-11 5.04e-07 3.24e-10 0.172 nd: 1.58700 Vd: 59.6 glass_code: 587596 density: 3.0 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.1e-06 K-1 dPgF: -0.0031 climatic_resistance: 2.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book