Optical constants of SUMITA - BaF (Barium flint)
K-BaFn3
Wavelength:
µm
(0.330 – 2.000)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.7128944-0.010619935λ^{2}+0.019653632λ^{-2}+0.00040051165λ^{-4}+1.1626539\text{×}10^{-06}λ^{-6}+1.1579589\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.44e-08 1.27e-08 -3.11e-10 5.72e-07 5.44e-10 0.214 nd: 1.66422 Vd: 49.2 glass_code: 664492 density: 3.62 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.5e-06 K-1 dPgF: -0.0024 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book