Optical constants of SUMITA - BaF (Barium flint)
K-BaF8
Wavelength:
µm
(0.340 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5830562-0.01131971λ^{2}+0.018817464λ^{-2}+0.00027063309λ^{-4}+2.1527561\text{×}10^{-05}λ^{-6}+7.7761941\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.3e-07 1.78e-08 -2.34e-10 5.81e-07 1.81e-11 0.234 nd: 1.62374 Vd: 47.1 glass_code: 624471 density: 3.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.8e-06 K-1 dPgF: 0.0001 climatic_resistance: 1.0 acid_resistance: 2.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book