Optical constants of SUMITA - BPG
K-BPG2
Wavelength:
µm
(0.330 – 2.000)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.3909284-0.0090241173λ^{2}+0.014036614λ^{-2}+0.00033108428λ^{-4}-9.985229\text{×}10^{-06}λ^{-6}+1.1070906\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 6.45e-06 1.89e-08 -2.11e-10 5.53e-07 8.99e-10 0.207 nd: 1.55920 Vd: 53.9 glass_code: 559539 density: 2.72 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.4e-06 K-1 dPgF: -0.0005 climatic_resistance: 1.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book