Optical constants of SUMITA - BOC
K-BOC30
Wavelength:
µm
(0.360 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.8354813-0.015056123λ^{2}+0.060329996λ^{-2}+0.002453809λ^{-4}+1.7392287\text{×}10^{-05}λ^{-6}+1.7174222\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.71e-06 1.58e-08 -2.57e-10 1.04e-06 1.1e-09 0.282 nd: 2.00680 Vd: 26.2 density: 4.8 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.5e-06 K-1 dPgF: 0.0099 climatic_resistance: 1.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book