Optical constants of SUMITA - BOC
K-BOC20
Wavelength:
µm
(0.36 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.8410887-0.015801048λ^{2}+0.055983447λ^{-2}+0.0030905124λ^{-4}-0.00016655999λ^{-6}+2.7794823\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -3.96e-07 1.14e-08 -3.48e-10 1e-06 9.73e-10 0.275 nd: 2.00540 Vd: 27.7 density: 4.95 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.5e-06 K-1 dPgF: 0.0064 climatic_resistance: 1.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book