RefractiveIndex.INFO

Refractive index database


Shelf

Book

Page

Optical constants of SCHOTT - Obsolete glasses
LF7

Wavelength: µm
 (0.334 – 0.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.26879731λ^2}{λ^2-0.00919553925}+\frac{0.156697051λ^2}{λ^2-0.0447256764}+\frac{0.887676301λ^2}{λ^2-106.8203610}$$

Comments

obsolete

References

SCHOTT LF7 glass data sheet (2006)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SCHOTT AG

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links


Glass

External links