Optical constants of SCHOTT - multiple purpose
LITHOSIL-Q (obsolete)
Wavelength:
µm
(0.25 – 2.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.67071081λ^2}{λ^2-0.00449192312}+\frac{0.433322857λ^2}{λ^2-0.0132812976}+\frac{0.877379057λ^2}{λ^2-95.8899878}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.06e-05 2.51e-08 -2.47e-11 3.12e-07 4.22e-10 0.16 nd: 1.45844E+00 Vd: 6.78300E+01 glass_code: 458678.220 glass_status: preferred density: 2.2 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5e-07 K-1 - temperature_range: 20 300 ℃ coefficient: 5.5e-07 K-1 dPgF: -0.0021 climatic_resistance: 1.0 stain_resistance: 0.0 acid_resistance: 1.0 alkali_resistance: 1.0 phosphate_resistance: 1.0
Comments
obsolet
References
SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)
See also SCHOTT glass data sheets