Optical constants of SCHOTT - SK (Dense crown)
N-SK2

Wavelength: µm
 (0.31 – 2.5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.28189012λ^2}{λ^2-0.0072719164}+\frac{0.257738258λ^2}{λ^2-0.0242823527}+\frac{0.96818604λ^2}{λ^2-110.377773}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 3.8e-06 1.41e-08 2.28e-11 6.44e-07 8.03e-11 0.108
nd: 1.60738
Vd: 56.65
glass_code: 607567.355
glass_status: standard
density: 3.55 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 6e-06 K-1
  - temperature_range: 20 300 °C
    coefficient: 7.1e-06 K-1
dPgF: -0.0008
climatic_resistance: 2.0
stain_resistance: 0.0
acid_resistance: 2.2
alkali_resistance: 1.0
phosphate_resistance: 2.3

Comments

step 0.5 available

References

SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)
See also SCHOTT glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SCHOTT AG

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links


Glass

External links