Optical constants of SCHOTT - SK (Dense crown)
N-SK15
Wavelength:
µm
(0.334 – 2.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.30417786λ^2}{λ^2-0.00695051276}+\frac{0.28584116λ^2}{λ^2-0.0232023703}+\frac{0.974781572λ^2}{λ^2-99.016884}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.92e-07 1.2e-08 -2.96e-12 4.66e-07 5.16e-10 0.179 nd: 1.62296 Vd: 58.02 glass_code: 623580.362 glass_status: special density: 3.62 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.7e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.6e-06 K-1 dPgF: -0.0009 climatic_resistance: 3.0 stain_resistance: 3.0 acid_resistance: 52.2 alkali_resistance: 2.0 phosphate_resistance: 3.2
Comments
inquiry glass
References
SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)
See also SCHOTT glass data sheets