Optical constants of SCHOTT - SF (Dense flint)
SFL6
Wavelength:
µm
(0.37 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.78922056λ^2}{λ^2-0.0135163537}+\frac{0.328427448λ^2}{λ^2-0.0622729599}+\frac{2.01639441λ^2}{λ^2-168.014713}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -5.26e-06 7.41e-09 -1.89e-11 1.02e-06 1.62e-09 0.288 nd: 1.80518 Vd: 25.39 glass_code: 805254.337 glass_status: special density: 3.37 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.03e-05 K-1 dPgF: 0.0148 climatic_resistance: 1.0 stain_resistance: 0.0 acid_resistance: 2.0 alkali_resistance: 1.0 phosphate_resistance: 1.0
Comments
inquiry glass
References
SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)
See also SCHOTT glass data sheets