$$n^2-1=\frac{1.88742326λ^2}{λ^2-0.0145939341}+\frac{0.360534025λ^2}{λ^2-0.0648198946}+\frac{2.26189313λ^2}{λ^2-176.062211}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.63e-06 8.61e-09 -9.98e-12 1.1e-06 1.69e-09 0.293 nd: 1.84666 Vd: 23.62 glass_code: 847236.355 glass_status: special density: 3.55 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 1e-05 K-1 dPgF: 0.0177 climatic_resistance: 1.0 stain_resistance: 0.0 acid_resistance: 1.3 alkali_resistance: 1.0 phosphate_resistance: 1.3
Comments
inquiry glass
References
SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)