Optical constants of SCHOTT - SF (Dense flint)
SF15
Wavelength:
µm
(0.37 – 2.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.53925927λ^2}{λ^2-0.0119307961}+\frac{0.247620926λ^2}{λ^2-0.0556077536}+\frac{1.03816409λ^2}{λ^2-116.416747}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.91e-06 1.69e-08 -3.77e-11 1.1e-06 1.07e-09 0.278 nd: 1.69895 Vd: 30.07 glass_code: 699301.406 glass_status: preferred density: 4.06 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.9e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.9e-06 K-1 dPgF: 0.0066 climatic_resistance: 1.0 stain_resistance: 0.0 acid_resistance: 1.0 alkali_resistance: 1.2 phosphate_resistance: 2.3
Comments
was replaced by N-SF15
References
SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)
See also SCHOTT glass data sheets