Optical constants of SCHOTT - SF (Dense flint)
N-SF1

Wavelength: µm
 (0.37–2.5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.60865158λ^2}{λ^2-0.0119654879}+\frac{0.237725916λ^2}{λ^2-0.0590589722}+\frac{1.51530653λ^2}{λ^2-135.521676}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -3.72e-06 8.05e-09 -1.71e-11 8.98e-07 1.34e-09 0.276
nd: 1.71736
Vd: 29.62
glass_code: 717296.303
glass_status: standard
density: 3.025 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 9.13e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.054e-05 K-1
dPgF: 0.0097
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

Comments

References

SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)
See also SCHOTT glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SCHOTT AG

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links


Glass

External links