Optical constants of SCHOTT - K (Crown)
N-ZK7A
Wavelength:
µm
(0.3 – 2.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.07509891λ^2}{λ^2-0.00676601657}+\frac{0.168895044λ^2}{λ^2-0.0230642817}+\frac{0.860503983λ^2}{λ^2-89.0498778}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.09e-05 1.98e-08 -1.49e-11 4.48e-07 3.26e-10 0.183 nd: 1.508054 Vd: 61.04 glass_code: 508610.247 glass_status: standard density: 2.4708 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 4.61e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 5.23e-06 K-1 dPgF: -0.0043 climatic_resistance: 1.0 stain_resistance: 0.0 acid_resistance: 2.0 alkali_resistance: 1.2 phosphate_resistance: 2.2
Comments
References
SCHOTT Zemax catalog 2017-01-20b (obtained from http://www.schott.com)
See also SCHOTT glass data sheets