Optical constants of SCHOTT - IRG
IRG 26
Wavelength:
µm
(0.85 – 15.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=3.1934+\frac{3.5854λ^2}{λ^2-0.1852}+\frac{2.2337λ^2}{λ^2-3398.08}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.63e-05 0 0 2.93e-05 0 3.15e-01 density: 4.63 g/cm3 thermal_expansion: - temperature_range: 20 100 °C coefficient: 21.4e-06 K-1 specific_heat: 0.36 J/(g·K) thermal_conductivity: - value: 0.24 W/(m·K) transition_temperature: 185 °C Knoop_hardness: 1.04 GPa fracture_toughness: 0.285 MPa·m1/2 Youngs_modulus: 18.3 GPa
References
SCHOTT Infrared Chalcogenide Glasses - IRG 26 Product flyer (Version April 2017)
Data
INFO
Infrared glass
Often, calcogenide glasses are used in the optical systems operating at infrared wavelengths ~1-14 µm (for instance, optical systems for thermal imaging and night vision)Infrared glass types/brands from different makers
- AMTIR (an acronym for "Amorphous Material Transmitting Infrared Radiation"): Amorphous Materials Inc. (AMI)
- IG: VITRON
- IRG: SCHOTT
- BD: LightPath
- OPTIR: Rochester Precision Optics (RPO)
Cross-reference
Composition | AMI | VITRON | SCHOTT | LightPath | RPO |
---|---|---|---|---|---|
Ge33As12Se55 | AMTIR-1 | IG 2 | IRG 22 | OPTIR-1* | |
Ge30Sb13Se32Te25 | IG 3 | IRG 23* | |||
Ge10As40Se50 | IG 4 | IRG 24 | |||
Ge28Sb12Se60 | AMTIR-3* | IG 5 | IRG 25 | BD-2 | OPTIR-3* |
As40Se60 | AMTIR-2 | IG 6 | IRG 26 | BD6 | |
As40S60 | AMTIR-6 | IRG 27 |
External Links
- Infrared - Wikipedia
- Chalcogenide glass - Wikipedia
- AMTIR amorphous material transmitting IR radiation - Amorphous Materials
- Brief introduction: chalcogenide glasses - VITRON
- Infrared Chalcogenide Glasses - SCHOTT
- Optical resources and technical information - LightPath